Grade : 55NiCrMoV7
Number:1.2714
Classification: Hot-work tool steel
Standard: EN ISO 4957: 2000 Tool steels
Low alloy special purpose steels or group L steels contain small quantities of chromium, nickel, vanadium, and molybdenum. L2 and L6 form the group L steels.
The L6 Die Block Steels contain 0.70% carbon with a quenched hardness of about 64 HRC. The alloying elements in these Die Block Steels are chromium and molybdenum, and 1.50% nickel to increase toughness. These Die Block Steel can maintain hardness above 60 HRC for sections of 75 mm (3 in.) thickness.
Diameter : 80 to 600 mm ;
Length : 1000 to 9000 mm ;
Delivery condition : Normalized, or Annealed, or Quenched and Tempered ;
Surface condition : Grounded, or Turned, or Polished
1. High Quality, Reasonable Price
2. Over 40 Years Experience
3. ISO NQA Certificated Factory
4. Worldwide shipping
5. Emergency Orders and Fast Delivery
Typically used in machine tool applications such as bearings, springs, rollers or chuck parts.
ASTM | DIN | UNI | JIS |
L6 | DIN 1.2714 | T61206 | SKT4 |
Steel Grade | C | Si | Mn | P | S | Cr | Ni | Mo | |
L6 | 0.65-0.75 | 0.10-0.50 | 0.25-0.80 | 0.030 max | 0.030 max | 0.60-1.20 | 1.25-2.00 | 0.50 max | / |
DIN1.2714 | 0.50-0.60 | 0.10-0.40 | 0.60-0.90 | 0.030 max | 0.030 max | 1.00-1.20 | 1.50-1.80 | 0.45-0.55 | 0.07-0.12 |
FORGING: L6 Die Block Steels are forged at 1079°C (1975°F) down to 871°C (1600°F). These steels should not be forged below 843°C (1550°F).
ANNEALING: Annealing must be performed after hot working and before re-hardening.
Heat at a rate not exceeding 400°F per hour (222°C per hour) to 1400°F (760°C), and hold at temperature for 1 hour per inch (25.4mm) of maximum thickness; 2 hours minimum. Then cool slowly with the furnace at a rate not exceeding 50°F per hour (28°C per hour) to 1000°F (538°C). Continue cooling to ambient temperature in the furnace or in air. The resultant hardness should be a maximum of 235 HBW.
For improved machinability, hold at 1400°F (760°C) for1 hour per inch (25.4mm) of maximum thickness; 2 hours minimum. Then cool slowly with the furnace cool from 1400°F (760°C) to 1250°F (677°C), hold for 8 hours, then air cool to ambient temperature. The resultant hardness should be a maximum of 192 HBW.
HARDENING: L6 Die Block Steels should be preheated at 1200°F, soaked, then raised to a hardening temperature of 1500 to 1550°F and held for one hour per inch of greatest cross section. Quench in oil to a temperature of 1500°F, followed immediately by tempering. Tools made of L6 Die Block Steels in sections less than 1 in. thickness are often air-quenched from 1500°F. Air quenching provides safer hardening of intricate sections. It also results in less distortion than oil quenching.
TEMPERING: L6 Die Block Steels should be tempered at 400°F. However, where increased toughness is desired, at a sacrifice of some hardness, higher tempering temperatures are often used.
L6 Die Block Steels do not become brittle, as many other die steels do, when tempered in the range of 450 to 800°F. A minimum holding time of one hour per inch of thickness should be used when tempering at 400°F.
To minimize the possibility of cracking, the steel should be tempered immediately after hardening and should be heated slowly to the desired tempering temperature.
For the tempering test of this grade, specimens 7/8 in. round by 2-1/2 in. long were hardened from 1500°F in air-blast furnace and from 1525°F in oil. The hardened specimens were tempered at temperatures ranging from 300 to 1000°F at 100-degree intervals.
Properties | Metric | Imperial |
Poisson’s ratio | 0.27-0.30 | 0.27-0.30 |
Elastic modulus | 190-210 GPa | 27557-30457 ksi |
EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.
1 EAF: Electric Arc Furnace
2 EAF+LF+VD: Refined-smelting and vacuum degassing
3 EAF+ESR: Electro Slag Remelting
4 EAF+PESR: protective atmosphere Electro Slag Remelting
5 VIM+PESR: Vacuum induction melting
1 Hot rolling process
2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
1 Black Surface
2 Grounded: Bright but rough ; Not precision
3 Machining for plate: Bright and precision; Little turning scar
4 Peeled/Turned: Bright and precision; Little turning scar
5 Polished: Very Bright and precision size; Not turning scar
1 Cutting: Small pieces
2 CNC Machine: Produce as your drawing
3 Package: Bare/Nylon/Canvas/Wooden
4 Payment:T/T, L/C, O/A(request credit)
5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)
网络文化经营许可证:浙网文[2013]0268-027号|增值电信业务经营许可证:浙B2-20080224-1 2007-2025 Tradevv.com. All rights reserved.